Preparation and properties of Al2O3-Fe2O3/3Y-TZP gradient composite ceramics with multilayer ceramic structure

  • In order to achieve a better close shade of artificial restoration match with natural dentition, a color-gradient 3 mol% Y2O3-stabilized ZrO2 (3Y-TZP) ceramics for dental restoration was prepared by forming and sintering process with powders of Fe2O3 (0.01wt%-0.09wt%)-Al2O3 (0.1wt%)/3Y-TZP as the raw materials. Their colorimetric characterization, sintering performance, and mechanical properties were tested, and the effect of Fe2O3 and Al2O3 on 3Y-TZP ceramics was studied. The results show that the color of the gradient Al2O3-Fe2O3/3Y-TZP changing from saffron yellow to white gradually, which matches with the natural dentition. In addition, the doping of trace Al2O3 (0.1wt%) on uncolored porcelain layer can avoid the cracking between porcelain layers during the presintering process. The flexural strength changes of gradient and can meet the need of dental restoration (≥ 800 MPa). The doping of trace Fe2O3 (0.01wt%) and Al2O3 (0.1wt%) can improve the densification and grain growth during the sintering process. And the doping of trace Fe2O3 (0.01wt%) and Al2O3 (0.1wt%) in 3Y-TZP can increase the flexural strength of the Al2O3-Fe2O3/3Y-TZP, but the flexural strength decreases when more Fe2O3 is doped (≤ 0.09wt%) in 3Y-TZP.
  • loading

Catalog

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return